Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 234.422 - 234.422 MPa @Temperature -40.0 - -40.0 °C |
34000.1 - 34000.1 psi @Temperature -40.0 - -40.0 °F |
Average value: 234 MPa Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Flexural Yield Strength | 70.0 - 234.422 MPa @Temperature -40.0 - 121 °C |
10200 - 34000.1 psi @Temperature -40.0 - 250 °F |
Average value: 113 MPa Grade Count:22 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |