Polymer Property : Flexural Yield Strength = 34000.1 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 234.422 - 234.422 MPa

@Temperature -40.0 - -40.0 °C
34000.1 - 34000.1 psi

@Temperature -40.0 - -40.0 °F
Average value: 234 MPa Grade Count:1
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..
Flexural Yield Strength 70.0 - 234.422 MPa

@Temperature -40.0 - 121 °C
10200 - 34000.1 psi

@Temperature -40.0 - 250 °F
Average value: 113 MPa Grade Count:22
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..