Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 261 MPa | 37900 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Flexural Yield Strength | 261 MPa | 37900 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Flexural Yield Strength | 261 - 352 MPa @Temperature -40.0 - 60.0 °C |
37900 - 51100 psi @Temperature -40.0 - 140 °F |
Average value: 154 MPa Grade Count:1 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
Flexural Yield Strength | 261 MPa | 37900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Verton PV007SV_WH8D537 PA 6 Preliminary data for 35% long fiber single pellet color filled PA6This data was supplied by SABIC-IP for the Americas region. |