Polymer Property : Flexural Yield Strength = 530 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 58.8 - 530 MPa
8530 - 76900 psi
Average value: 261 MPa Grade Count:531
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Flexural Yield Strength 180 - 530 MPa
26100 - 76900 psi
Average value: 331 MPa Grade Count:50
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..