Mechanical Properties Metric English Comments
Flexural Yield Strength 58.8 - 530 MPa
8530 - 76900 psi
Average value: 261 MPa Grade Count:531
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Flexural Yield Strength 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID HI5006A(W) PA6/ABS, High Impact, Good Dimensional Stability
Feature: Injection Molding, PA6/ABS, High Impact, Good Dimensional StabilityApplication: Pipe Fitting, Electrical and Electronic partsCAS No. 25038-54-4, 9003-56-9 and 9003-54-7Information provided ..
Flexural Yield Strength 58.8 MPa
8530 psi
ASTM D790
IRPC Polimaxx Polene 2311LCX GA4 Polypropylene Compound
CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 20% GLASS FIBRE REINFORCED, HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, HIGH STIFFNESS, LOW SHRINKAGEAPPLICATIONS: INJECTION MOLDING FOR AUTOP..
Flexural Yield Strength 58.8 MPa
8530 psi
ASTM D790
Samyang Trimma® SD6320P PMMA, Translucent
High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Information provided by Samyang.
Flexural Yield Strength 58.8 MPa

@Temperature 260 °C
8530 psi

@Temperature 500 °F
ASTM D790
UBE UPIMOL® R Polyimide Shape
Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub..
Flexural Yield Strength 58.8 MPa
8530 psi
ASTM D790
Cheng Yu Plastic PP230H TALC 30 Polypropylene, 30% Talc, High Heat
Flexural Yield Strength 58.8 MPa

@Thickness 6.40 mm
8530 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron AN450N Flame Retardant ABS
Flame Retardant- V0 at 2.0mmInformation provided by Bhansali
Flexural Yield Strength 58.8 MPa

@Thickness 6.40 mm
8530 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade
High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali
Flexural Yield Strength 58.8 MPa

@Thickness 6.40 mm
8530 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IM-17 A EP ABS Electro Plating Applications
Electroplating & Hot Stamping GradesInformation provided by Bhansali
Flexural Yield Strength 58.8 MPa

@Thickness 6.40 mm
8530 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade
High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali
Flexural Yield Strength 58.8 MPa
8530 psi
ASTM D790
Cheng Yu Plastic IPS610BK Electric Conducting HIPS, Extrusion
Flexural Yield Strength 58.8 MPa

@Thickness 6.40 mm
8530 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS
Flame Retardant- IS 15061 conformedInformation provided by Bhansali
Flexural Yield Strength 58.8 MPa

@Thickness 6.40 mm
8530 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron AN450N Flame Retardant ABS
Flame Retardant- V0 at 2.0mmInformation provided by Bhansali
Flexural Yield Strength 58.8 MPa

@Thickness 6.40 mm
8530 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IM-17 A EP ABS Electro Plating Applications
Electroplating & Hot Stamping GradesInformation provided by Bhansali
Flexural Yield Strength 58.8 MPa

@Thickness 6.40 mm
8530 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS
Flame Retardant- IS 15061 conformedInformation provided by Bhansali