Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycolac® X15 ABS Automotive. Very high heat resistance with high impact. UL94 HB rated. High gloss.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC8100 PC+ABS Extrusion blowmolding grade. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC8100 PC+ABS (Asia Pacific) Extrusion blowmolding grade. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Geloy EXGY30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Geloy FXTW30PE ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | ISO 178 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
LG Chemical LG-703A ABS, Low Gloss, General Purpose Information Provided by LG Chem |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP GL003XXP PSU (Europe-Africa-Middle East) LNP* LUBRICOMP* GL003XXP is a compound based on Polysulfone resin containing PTFE. Added features include; Internally Lubricated. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 308 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 309 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500. Available in Natural (1001) only. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® ENH3500 PBT (Asia Pacific) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® 1103 PBT+PC AUTOMOTIVE. Unreinforced, impact modified PBT+PC alloy. Excellent low temperature impact and chemical resistance. Range gray, black colors. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Europe-Africa-Middle East) LNP* STAT-KON* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containg Carbon Fiber. Added features include: Electrically Conductive |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® ENH3500 PBT (Europe-Africa-Middle East) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® SLWM2105 PBT+PC (Asia Pacific) Anti-static PBT/PC blend, mineral 5% filled productThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY SLWM2105 PBT+PC (Asia Pacific) Anti-static PBT/PC blend, mineral 5% filled product |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | ISO 178 |
Eastman Eastar EN001 Copolyester Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Asia Pacific) Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Asia Pacific) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |