Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP GL003XXP PSU (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP GL003XXP PSU (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* GL003XXP is a compound based on Polysulfone resin containing PTFE. Added features include; Internally Lubricated.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
5 mm/min; ISO 527
Elongation at Break 6.0 - 8.0 %
6.0 - 8.0 %
5 mm/min; ISO 527
Tensile Modulus 1.80 GPa
261 ksi
1 mm/min; ISO 527
Flexural Yield Strength 77.0 MPa
11200 psi
2 mm/min; ISO 178
Flexural Modulus 2.40 GPa
348 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 70.0 kJ/m²
33.3 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-1

@Thickness 0.800 mm
V-1

@Thickness 0.0315 in
UL 94
Users viewing this material also viewed the following: