Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
ExxonMobil Exceed™ 3518 GA Premium Cast Film Resin
(discontinued **) Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
LyondellBasell Petrothene® NA443023 Blown Low Density Polyethylene ApplicationsPETROTHENE NA 443 is a series of low density/EVA copolymer resins for high impact/high clarity packaging applications. NA 443 exhibits excellent processability and good balance of optic.. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
Westlake DA591 9.0% Ethylene Vinyl Acetate Copolymer Westlake DA591 resin is a 9.0% EVA copolymer designed as a tie layer in multi-layered food packaging film. It has excellent clarity, excellent toughness, good resistance to load deformation, and goo.. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | D 882 |
Westlake EB591 9.0% Ethylene Vinyl Acetate Copolymer Westlake EB591 resin is a 9.0% EVA copolymer designed for ice bags, frozen food bags and other films that require excellent toughness and good heat sealing characteristics. This kosher compliant re.. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM-D882 |
Westlake Elevate™ EB591 9% EVA Copolymer Westlake EB591 resin is a 9% EVA copolymer designed for films that require excellent toughness and good heat sealing characteristics. This Kosher compliant resin has excellent low temperature brittl.. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
ExxonMobil Escorene® LD 701.ID Blown Film Resin Escorene Ultra LD 701.ID is a fraction melt index, 10.5 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particularly.. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012HA Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes.. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
ExxonMobil Exceed™ 4518PA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 4581PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 4581PA have outstanding tensile properties and impact and puncture toughness. These superior prope.. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
ExxonMobil Exceed™ 4518PA Premium Cast Film Resin Exceed 4518PA resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 4518PA resin have outstanding tensile properties and impact and puncture toughness.. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
ExxonMobil LDPE LD 331.08 Low Density Polyethylene Resin Product Description: LD 331.08 is a 5.9% vinyl acetate copolymer, higher clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Availability: Latin Amer.. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
ExxonMobil LL 3003.32 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
ExxonMobil LL 3003.39 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3003.32 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3003.39 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012HJ Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes.. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
ExxonMobil Exceed™ 3518 CB Premium Cast Film Resin Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
ExxonMobil Exceed™ 3518 PA Premium Cast Film Resin Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
1% Secant Modulus, TD | 124 MPa | 18000 psi | ASTM D882 |
ExxonMobil Exceed™ 4518CB Metallocene Polyethylene Resin Product Description: Exceed 4518 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 4518 have outstanding tensile properties and impact and puncture toughness. These superior p.. |