Mechanical Properties Metric English Comments
Tensile Modulus 11.0 GPa

@Temperature 23.0 °C
1600 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym..
Tensile Modulus 11.0 GPa

@Temperature 23.0 °C
1600 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66  (Unverified Data**)
Zytel® LM70G35HSLX is a 35% glass fiber reinforced, heat stabilized, lubricated polyamide 66 for injection molding. It is well suited for laser marking.Information provided by DuPont Performance Po..
Tensile Modulus 11.0 GPa

@Temperature 23.0 °C
1600 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6  (Unverified Data**)
Zytel® 73G35HSL BK262 is a 35% glass fiber reinforced, heat stabilized, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 11.0 GPa

@Temperature 90.0 °C
1600 ksi

@Temperature 194 °F
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 11.0 GPa

@Temperature 23.0 °C
1600 ksi

@Temperature 73.4 °F
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin..
Tensile Modulus 11.0 GPa

@Temperature 60.0 °C
1600 ksi

@Temperature 140 °F
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Modulus 11.0 GPa

@Temperature 23.0 °C
1600 ksi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/35-V0KB1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Modulus 11.0 GPa

@Temperature 60.0 °C
1600 ksi

@Temperature 140 °F
LATI Latamid 66 H2 G/50-GWHF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. improved G.W.F.I. compared to standard product.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
Tensile Modulus 11.0 GPa

@Temperature 120 °C
1600 ksi

@Temperature 248 °F
LATI Latamid 66 H2 K/40 PA 66, 40% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Modulus 11.0 GPa

@Temperature 90.0 °C
1600 ksi

@Temperature 194 °F
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 11.0 GPa

@Temperature 150 °C
1600 ksi

@Temperature 302 °F
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 11.0 GPa

@Temperature 23.0 °C
1600 ksi

@Temperature 73.4 °F
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Tensile Modulus 11.0 GPa

@Temperature 60.0 °C
1600 ksi

@Temperature 140 °F
LATI Latene® AG7H K/30 PP Homopolymer, 30% Carbon Fiber Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Carbon fiber. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Tensile Modulus 11.0 GPa

@Temperature 120 °C
1600 ksi

@Temperature 248 °F
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced
Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: ..
Tensile Modulus 11.0 GPa

@Temperature 90.0 °C
1600 ksi

@Temperature 194 °F
LATI Latigloss 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Modulus 11.0 GPa

@Temperature 23.0 °C
1600 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® PLUS PLS95G35DH1 BK031 Nylon
Zytel® PLS95G35DH1 BK031is a high flow 35% glass reinforced PA using SHIELD Technology, only from DuPont, combining excellent surface appearance, excellent welding and fatigue retention, exceptiona..
Tensile Modulus 11.0 GPa

@Temperature 23.0 °C
1600 ksi

@Temperature 73.4 °F
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.Avail..
Tensile Modulus 11.0 GPa

@Temperature 23.0 °C
1600 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66  (Unverified Data**)
Zytel® 70G43HSLA BK099 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers