Polymer Property : Tensile Modulus = 203 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.40 GPa

@Temperature 23.0 °C
203 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66  (Unverified Data**)
Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Modulus 1.40 GPa

@Temperature 23.0 °C
203 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66  (Unverified Data**)
Zytel® 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 1.40 GPa

@Temperature 23.0 °C
203 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66  (Unverified Data**)
Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 1.40 GPa

@Temperature 23.0 °C
203 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 1.40 GPa

@Temperature 120 °C
203 ksi

@Temperature 248 °F
Hybrid Plastics Nanoreinforced® Cellulose Propionate Acetate
Nanoreinforced® Cellulose Propionate Acetate is an optically clear nanocomposite with POSS® dispersed at the nanometer level. Compared to virgin cellulose propionate acetate, it enhances mecha..
Tensile Modulus 1.40 GPa

@Temperature 60.0 °C
203 ksi

@Temperature 140 °F
LATI Latamid 6 H-V0 PA 6, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good surface appearance.Availability: Africa & Middle East; Asi..
Tensile Modulus 1.40 GPa

@Temperature 60.0 °C
203 ksi

@Temperature 140 °F
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin ..
Tensile Modulus 1.40 GPa

@Temperature 23.0 °C
203 ksi

@Temperature 73.4 °F
LATI Latene® 7-V2 PP Homopolymer, Flame Retardant
Polypropylene homopolymer (PPh) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
Tensile Modulus 1.40 GPa

@Temperature 60.0 °C
203 ksi

@Temperature 140 °F
LATI Latan 23UVE71 POM
Polyoxymethylene (POM). UV stabilized. Toughened. Low viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati..
Tensile Modulus 1.40 GPa

@Temperature 60.0 °C
203 ksi

@Temperature 140 °F
LATI Latan 9 POM
Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La..
Tensile Modulus 1.40 GPa

@Temperature 50.0 °C
203 ksi

@Temperature 122 °F
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Tensile Modulus 1.40 GPa

@Temperature 23.0 °C
203 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66  (Unverified Data**)
Zytel® FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applications such as parts for the food industry.Information provided by D..
Tensile Modulus 1.40 GPa

@Temperature 60.0 °C
203 ksi

@Temperature 140 °F
LATI Latiblend 7587 E61-V0 PBT/PC, Flame Retardant
Blend based on Polybutylene Terephthalate (PBT) / Polycarbonate (PC). Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. High impact re..