Polymer Property : Compressive Strength = 30.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1000 °C
2900 - 4350 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 110 C Dense Refractory Castable
Description: Curon 110 C is a coarse castable. Application: covers for anode baking furnaces.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1000 °C
2900 - 4350 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 120 C Dense Refractory Castable
Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 C has good thermal shock resistance.Remarks: These values apply to cast products.Informat..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 100 °C
2900 - 4350 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 120 LC AL Dense Refractory Castable
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1000 °C
2900 - 4350 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 120 LC AL Dense Refractory Castable
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 100 °C
2900 - 4350 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 145 F Sp Dense Refractory Castable
Description: Curon 145F Special is a very fine graded castable and can be applied for the casting of complicated shapes.Remarks: These values apply to cast products. Also available in gunning variet..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1000 °C
2900 - 4350 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 127 S GM Dense Refractory Castable
Description: Curon 127 S GM gunning castable is characterized by a reasonable strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks:..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1400 °C
2900 - 4350 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 GM Dense Refractory Castable
Description: Curon 150 GM is a gunmix based on sintered bauxite with an excellent thermal shock resistance and is therefore very well suited for burner blocks.Remarks: These values apply to cast pro..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1000 °C
2900 - 4350 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 100 C Dense Refractory Castable
Description: Curon 100 C can be applied up to 1000°C, under normal operating conditions and is especially applied in the bottom of electrolytic cells in the aluminum industry.Remarks: These values ..
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1300 °C
2900 - 4350 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 165 GM Dense Refractory Castable
Description: Curon 165 GM is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Other mo..