Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® JK2000 PC+ABS (Asia Pacific) Lexan* JK2000 compound is a glass reinforced, non-Br and non-Cl FR polycarbonate blends designed for thinwall molding applications. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP GFL36L PSU (Asia Pacific) LNP* Lubricomp* GFL36L is a compound based on Polysulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 2210EPR PEI 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DEF42 PC LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DX02728C PC LNP STAT-KON* DX02728C is a compound based on Polycarbonate resin containing Proprietary Filler(s) Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON Lexan_JK2500 PC+ABS LNP* Stat-kon* Lexan_JK2500 compound is a 20% carbon-fiber reinforced, nonhalogenated red phosporous-free, high-flow FR PC+ABS for EMI/RFI shielding. SE of 21 dB at 1.5 mm. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS LNP* STAT-LOY* A30009 is a compound based on ABS. Added features of this material include: Antistatic, Flame Retardant. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS LNP* THERMOCOMP* AF003 is a compound based on ABS resin containing 15% Glass Fiber. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features include: Electrically Conductive, Easy Molding, Mold Release. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK2000 PC+ABS LNP* Thermocomp* Lexan_JK2000 compound is a 22% GR, ECO-compliant FR, PC+ABS for thinwall molding applications. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK (Asia Pacific) LNP* Thermocomp* LF003 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK (Asia Pacific) LNP* Thermocomp* LF005 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Asia Pacific) LNP* Thermocomp* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PH0240A PA 6 LNP* THERMOCOMP* PH0240A is a compound based on Nylon 6 resin. Added features of this grade include: High Impact, High Specific Gravity. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6 LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6 4.0 specific gravity, Nylon 6 |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS (Asia Pacific) LNP* Thermocomp* ZF0049 is a compound based on PPE+PS Blend resin containing Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Asia Pacific) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Europe-Africa-Middle East) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP 2C004 ETFE LNP* THERMOCOMP* 2C004 is a compound based on ETFE resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON RVL28 PA 66 LNP* VERTON* RVL28 is a compound based on Nylon 66 resin containing 40% Long Glass Fiber, 10% PTFE. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant, Structura.. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific) LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Dart Drop, Total Energy | 14.0 J @Thickness 0.0500 mm |
10.3 ft-lb @Thickness 0.00197 in |
1100N; ISO 7765-2 |
Borealis HD244CF Polypropylene HD244CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: food packaging, lamination films, stationery folders, multi layer co-extr.. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON NV006E PC/ABS (Asia Pacific) LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Dart Drop, Total Energy | 14.0 - 25.0 J @Temperature -29.0 - -29.0 °C |
10.3 - 18.4 ft-lb @Temperature -20.2 - -20.2 °F |
Average value: 18.3 J Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP GFL36L PSU LNP* Lubricomp* GFL36L is a compound based on Polysulfone resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |