Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP JFL34 PES LNP* LUBRICOMP* JFL34 is a compound based on Polyethersulfone resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 2210EPR PEI 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DX02728C PC LNP STAT-KON* DX02728C is a compound based on Polycarbonate resin containing Proprietary Filler(s) Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific) LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON Lexan_JK2500 PC+ABS LNP* Stat-kon* Lexan_JK2500 compound is a 20% carbon-fiber reinforced, nonhalogenated red phosporous-free, high-flow FR PC+ABS for EMI/RFI shielding. SE of 21 dB at 1.5 mm. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Asia Pacific) LNP* Stat-loy* A30009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS LNP* THERMOCOMP* AF003 is a compound based on ABS resin containing 15% Glass Fiber. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA 6/12 LNP THERMOCOMP* IF006 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK LNP* THERMOCOMP* LF003 is a compound based on Polyetheretherketone resin containing 15% Glass Fiber. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK (Asia Pacific) LNP* Thermocomp* LF003 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Asia Pacific) LNP* Thermocomp* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PH0240A PA 6 LNP* THERMOCOMP* PH0240A is a compound based on Nylon 6 resin. Added features of this grade include: High Impact, High Specific Gravity. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6 LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Europe-Africa-Middle East) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy .. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP 2C004 ETFE LNP* THERMOCOMP* 2C004 is a compound based on ETFE resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RC006H PA 66 LNP THERMOCOMP* RC006H is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS LNP* THERMOCOMP* ZF0049 is a compound based on PPE+PS resin containing 20% Glass Fiber. Added feature of this material is: Flame Retardant. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific) LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL EM7430 PPE+PS 30% glass reinforced, high flow PPO. Automotive. Energy management material. |
|||
Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Dart Drop, Total Energy | 14.0 J @Thickness 0.0500 mm |
10.3 ft-lb @Thickness 0.00197 in |
1100N; ISO 7765-2 |
Borealis HD234CF Polypropylene HD234CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD234CF is recommended for food packaging, lamination films, stationery f.. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON NV006E PC/ABS (Asia Pacific) LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP GFL36L PSU LNP* Lubricomp* GFL36L is a compound based on Polysulfone resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Dart Drop, Total Energy | 14.0 J | 10.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON NV006E PC+ABS LNP* Verton* NV006E is a compound based on PC+ABS blend resin containing 30% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |