SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS (Asia Pacific)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC+ABS, excellent flow/impact/high heat resistance. Suitable for thin wall application. Low temperature ductility (-20F). For automotive, appliance and electrical components.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 260 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
12 g/10 min

@Load 3.80 kg,
Temperature 260 °C
12 g/10 min

@Load 8.38 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 59.0 MPa
8560 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 75 %
75 %
Type I, 50 mm/min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 2.20 GPa
319 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 86.0 MPa
12500 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.37 GPa
344 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
2.67 J/cm

@Temperature -30.0 °C
5.00 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Dart Drop, Total Energy 61.0 J
45.0 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
47.0 J

@Temperature -30.0 °C
34.7 ft-lb

@Temperature -22.0 °F
Instrumented Impact Energy @ peak; ASTM D3763
54.0 J

@Temperature -30.0 °C
39.8 ft-lb

@Temperature -22.0 °F
ASTM D3763
61.0 J

@Temperature 23.0 °C
45.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
40.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 126 °C

@Thickness 3.20 mm
259 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C

@Thickness 3.20 mm
230 °F

@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 60.0 °C
140 °F
UL 746B
UL RTI, Mechanical with Impact 60.0 °C
140 °F
UL 746B
UL RTI, Mechanical without Impact 60.0 °C
140 °F
UL 746B
Flammability, UL94 HB

@Thickness 1.21 mm
HB

@Thickness 0.0476 in
UL 94
Electrical Properties Metric English Comments
Arc Resistance 120 - 180 sec
120 - 180 sec
Tungsten; ASTM D495
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
>= 120 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746A
Descriptive Properties Value Comments
UV-light, water exposure/immersion F2
UL 746C