Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3.03 - 17.0 MPa | 440 - 2470 psi | Average value: 10.2 MPa Grade Count:17 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported.. |
|||
Tensile Strength, Ultimate | 7.00 - 17.0 MPa @Temperature 250 - 250 °C |
1020 - 2470 psi @Temperature 482 - 482 °F |
Average value: 11.0 MPa Grade Count:8 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 5.00 - 17.0 MPa | 725 - 2470 psi | |
ATG s.r.l. FPM Fluoroelastomer |