Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.03 - 17.0 MPa
440 - 2470 psi
Average value: 10.2 MPa Grade Count:17
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..
Tensile Strength, Ultimate 7.00 - 17.0 MPa

@Temperature 250 - 250 °C
1020 - 2470 psi

@Temperature 482 - 482 °F
Average value: 11.0 MPa Grade Count:8
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max..
Tensile Strength, Ultimate 5.00 - 17.0 MPa
725 - 2470 psi
ATG s.r.l. FPM Fluoroelastomer