Polymer Property : Tensile Strength, Ultimate = 3700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 25.5 MPa
3700 psi
2 in/min.; ASTM D638
Ineos H20A-00 Polypropylene Homopolymer
A controlled rheology polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications requiring a moderate level of antistatic ag..
Tensile Strength, Ultimate 25.5 MPa
3700 psi
Kraton® D1102 + PP blend (25/75)
Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the ..
Tensile Strength, Ultimate 25.5 MPa
3700 psi
ASTM D638
KKPC Kuhmo HI 425 General Purpose HIPS
Key features: High-impact General Use. Common Uses: Office appliances, home appliances, various kitchenware, general merchandise, toys, leisure goods, etc.HIPS is a functional resin made by copolym..
Tensile Strength, Ultimate 25.5 MPa
3700 psi
ASTM D638
KKPC Kuhmo HI 425TVL High Flow/High Heat Resistant HIPS
Key features: Super high-fluidity. Common Uses: TV cover (Fine TV), Drawers.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-..
Tensile Strength, Ultimate 25.5 MPa
3700 psi
ASTM D638
American Polymers API 550 HF Polystyrene
API 550 HF is a high impact grade of polystyrene. It is characterized by good impact and processability. API 550 HF offers good retention of mechanical properties in applications with long flow le..
Tensile Strength, Ultimate 25.5 MPa
3700 psi
ASTM D638
DuPont™ Surlyn® 9520 Ionomer Resin, Zinc
Surlyn® 9520 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Tensile Strength, Ultimate 25.5 MPa
3700 psi
ASTM Data
Dow Retain® PS-4378 Polystyrene
Data provided by Dow Chemical.
Tensile Strength, Ultimate 25.5 MPa
3700 psi
ASTM D638
Colorite Polymers 1194B General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 25.5 MPa
3700 psi
Bond strength to glass
Dymax Light Weld® 401 High Clarity Glass Bonding Adhesive
Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond..
Tensile Strength, Ultimate 25.5 MPa
3700 psi
ASTM D638
Adell EZ-16 Homopolymer Polypropylene, 30% Calcium Carbonate Filled
Data provided by Adell Plastics, Inc.
Tensile Strength, Ultimate 25.5 MPa
3700 psi
0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638
Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin
STYRON™ 487 is a high-impact polystyrene with an excellent balance of flow, toughness, stiffness and heat resistance. It has excellent deep draw characteristics and is appropriate for extrusion ap..
Tensile Strength, Ultimate 25.5 MPa
3700 psi
ACMA Test #4
CeramTec 547 Cordierite (2MgO-2Al2O3-5SiO2)
Te value is 670°C. Hasselman Thermal Shock value is 800 K.Data provided by CeramTec North America.
Tensile Strength, Ultimate 25.5 MPa
3700 psi
ASTM D638
Adell RA-18 Copolymer Polypropylene, 40% Talc Filled
Data provided by Adell Plastics, Inc.
Tensile Strength, Ultimate 25.5 - 65.5 MPa
3700 - 9500 psi
Average value: 43.7 MPa Grade Count:9
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA)
This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max..