Polymer Property : Tensile Strength, Ultimate = 510 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 380 - 510 MPa
55100 - 74000 psi
Materion Brush 1915â„¢ Hard Temper Rod, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Tensile Strength, Ultimate 340 - 510 MPa
49300 - 74000 psi
Materion Brush 1915â„¢ Hard Temper Wire, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Tensile Strength, Ultimate 410 - 510 MPa
59500 - 74000 psi
SSAB Tunnplat Docol® 350YP High-strength Steel
High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report..
Tensile Strength, Ultimate 390 - 510 MPa
56600 - 74000 psi
SSAB Tunnplat Domex® 315MC HSLA Steel
HSLA SteelCharacteristics: For hot-dip galvanizing, a thin Zn coating (50-80 microns) is specified.Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better pr..
Tensile Strength, Ultimate 421 - 510 MPa
61000 - 74000 psi
Eagle Brass 18665 MSP1, 1/2 Hard
MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs..
Tensile Strength, Ultimate 441 - 510 MPa
64000 - 74000 psi
Eagle Brass 260 Cartridge Brass, 3/4 Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Tensile Strength, Ultimate 427 - 510 MPa
62000 - 74000 psi
Eagle Brass 425 Tin Brass 2%, 3/4 Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Tensile Strength, Ultimate 470 - 510 MPa
68200 - 74000 psi
L direction
ArcelorMittal Torque 20-15 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..
Tensile Strength, Ultimate 470 - 510 MPa
68200 - 74000 psi
L direction
ArcelorMittal Torque 25-16 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..
Tensile Strength, Ultimate 470 - 510 MPa
68200 - 74000 psi
L direction
ArcelorMittal Torque 27-16 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..
Tensile Strength, Ultimate 470 - 510 MPa
68200 - 74000 psi
L direction
ArcelorMittal Torque 30-17 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..
Tensile Strength, Ultimate 470 - 510 MPa
68200 - 74000 psi
L direction
ArcelorMittal Torque 30-18 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..
Tensile Strength, Ultimate 450 - 510 MPa
65300 - 74000 psi
ArcelorMittal FB 450 Hot rolled ferrite-bainite steel
Available in the following: uncoated (HDT450F) and Extragal® (HDT450F+Z)Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It compr..