Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 380 - 510 MPa | 55100 - 74000 psi | |
Materion Brush 1915â„¢ Hard Temper Rod, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Tensile Strength, Ultimate | 340 - 510 MPa | 49300 - 74000 psi | |
Materion Brush 1915â„¢ Hard Temper Wire, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Tensile Strength, Ultimate | 410 - 510 MPa | 59500 - 74000 psi | |
SSAB Tunnplat Docol® 350YP High-strength Steel High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report.. |
|||
Tensile Strength, Ultimate | 390 - 510 MPa | 56600 - 74000 psi | |
SSAB Tunnplat Domex® 315MC HSLA Steel HSLA SteelCharacteristics: For hot-dip galvanizing, a thin Zn coating (50-80 microns) is specified.Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better pr.. |
|||
Tensile Strength, Ultimate | 421 - 510 MPa | 61000 - 74000 psi | |
Eagle Brass 18665 MSP1, 1/2 Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Tensile Strength, Ultimate | 441 - 510 MPa | 64000 - 74000 psi | |
Eagle Brass 260 Cartridge Brass, 3/4 Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Tensile Strength, Ultimate | 427 - 510 MPa | 62000 - 74000 psi | |
Eagle Brass 425 Tin Brass 2%, 3/4 Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Strength, Ultimate | 470 - 510 MPa | 68200 - 74000 psi | L direction |
ArcelorMittal Torque 20-15 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Ultimate | 470 - 510 MPa | 68200 - 74000 psi | L direction |
ArcelorMittal Torque 25-16 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Ultimate | 470 - 510 MPa | 68200 - 74000 psi | L direction |
ArcelorMittal Torque 27-16 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Ultimate | 470 - 510 MPa | 68200 - 74000 psi | L direction |
ArcelorMittal Torque 30-17 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Ultimate | 470 - 510 MPa | 68200 - 74000 psi | L direction |
ArcelorMittal Torque 30-18 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Ultimate | 450 - 510 MPa | 65300 - 74000 psi | |
ArcelorMittal FB 450 Hot rolled ferrite-bainite steel Available in the following: uncoated (HDT450F) and Extragal® (HDT450F+Z)Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It compr.. |