Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638-61T |
Rotuba 860M Ethyl Cellulose Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 34.0 - 68.0 MPa | 4930 - 9860 psi | Average value: 55.1 MPa Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Tensile Strength, Ultimate | 34.0 MPa @Temperature 900 °C |
4930 psi @Temperature 1650 °F |
|
Resistalloy International Fecralloy™ 145 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kiln.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 Type IV |
Chevron Phillips Marlex® HHM TR-480Z/M362 Natural high density ethylene hexene copolymer/black concrete
(disc Benefits: good long term hoop strength performance, very high melt strength, outstanding toughness even at low temperatures, concrete base resinCharacteristics: Pipe Ring ESCR > 2000 h, ASTM F 1248;.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Chevron Phillips HiD® 9308 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 345460A; ASTM D 4976 Classification: PE 235, A 56607Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Chevron Phillips HiD® 9326 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 335440A; ASTM D 4976 Classification: PE 235, A 56606Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Chevron Phillips HiD® 9396T HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601Applications:Base Resin for use in Utility and Conduit Pipe ApplicationsData provided by.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
PolyOne Stat-Tech™ AS-15CP/000 ABS - 15% Carbon Powder
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
PolyOne Lubri-Tech™ ATH-000/05M Acetal Homopolymer - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 34.0 - 138 MPa | 4930 - 20000 psi | Average value: 76.3 MPa Grade Count:61 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Tensile Strength, Ultimate | 34.0 MPa @Temperature 60.0 °C |
4930 psi @Temperature 140 °F |
ISO 527 |
LATI LATILUB 82-01M Nylon 12 Base, 1% Molybdenum Disulfide Self Lubricating Plastic
(discontinued **) Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | |
Kuraray HYBRAR® PH6 Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
LyondellBasell Astryn SB572C Polypropylene Copolymer Key Features: fractional melt flow, medium modulus, extrusion grade polypropylene copolymer, good melt strength, good processabilityApplications: solar panelsDescription: Astryn SB572C fractional me.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Sumitomo Bakelite North America FM 4005X4648 Fiberglass Reinforced Phenolic Novolac FM 4005X4648 a fiberglass reinforced phenolic novolac molding compound formulated to increase thermal conductivity and electrical conductance. This material also exhibits low post mold shrinkage.In.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | 20 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1185 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | 20 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1185 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Plenco 1500 Polyester, Granular, Compression Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | 20 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1185 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Chevron Phillips Marlex® 9346 HDPE Natural Pipe Resin Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification:345464C when used with an approved color concentrate; ASTM D 4976 Classification: PE 235, A 56607Applications:Pressure Pip.. |
|||
Tensile Strength, Ultimate | 34.0 MPa @Temperature 871 °C |
4930 psi @Temperature 1600 °F |
|
AK Steel 18 SR® Ferritic Stainless steel AK Steel 18 SR® provides excellent resistance to high temperature scaling - far superior to that of Type 446 stainless steel. This material is readily welded by conventional methods. It is not su.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D412 |
BASF Elastollan® S85A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fue.. |
|||
Tensile Strength, Ultimate | 34.0 MPa | 4930 psi | ASTM D638 |
Toyobo E1080A Thermoplastic Polyurethane Elastomer, Extrusion Grade Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,.. |
|||
Tensile Strength, Ultimate | 34.0 MPa @Temperature 900 °C |
4930 psi @Temperature 1650 °F |
|
Resistalloy International Fecralloy™ 135 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire, bar, and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small .. |
|||
Tensile Strength, Ultimate | 34.0 MPa @Temperature 90.0 °C |
4930 psi @Temperature 194 °F |
ISO 527 |
LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |