Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 17.0 - 827 MPa | 2470 - 120000 psi | Average value: 79.8 MPa Grade Count:368 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Tensile Strength, Ultimate | 689 - 827 MPa | 100000 - 120000 psi | |
Meehanite HSV Heat Resisting Cast Iron Type HSV is an iron developed essentially for engineering parts subjected to long continuous heating. It has been designed to have the maximum load bearing ability.General Meehanite information - M.. |
|||
Tensile Strength, Ultimate | 621 - 827 MPa | 90000 - 120000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed Rod and Bar specifically. Other property values are typical of ann.. |
|||
Tensile Strength, Ultimate | 621 - 827 MPa | 90000 - 120000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Strip Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 3.. |
|||
Tensile Strength, Ultimate | 621 - 827 MPa | 90000 - 120000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Wire Tensile strength (ultimate) and elongation values reported here are typical for Annealed Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gen.. |
|||
Tensile Strength, Ultimate | 724 - 827 MPa | 105000 - 120000 psi | |
Eagle Brass 70265 XP175, 3/4 Hard Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 745 - 827 MPa | 108000 - 120000 psi | |
Eagle Brass 770 Nickel Silver 18%, Spring 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Strength, Ultimate | 689 - 827 MPa | 99900 - 120000 psi | |
Ametek AM 388™ Alloy (UNS C72650) TM00 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |