Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 70.0 MPa | 10200 psi | Estimated from similar grades.; ASTM D732 |
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Shear Strength | 70.0 MPa | 10200 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, at 50% RH
(disco AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Shear Strength | 70.0 MPa | 10200 psi | ASTM D732 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re.. |
|||
Shear Strength | 70.0 MPa | 10200 psi | ASTM D732 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
(Unverified Data**) AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot.. |
|||
Shear Strength | 70.3 MPa | 10200 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte.. |
|||
Shear Strength | 70.0 MPa @Thickness >=5.00 mm |
10200 psi @Thickness >=0.197 in |
Parallel to laminations; EN 60893 |
HOS-Technik Homide 250 Bismaleimide Resin Homide 250 is a prepolymer bismaleimide resin system with a low softening range of 90-125°C supplied in powder form. The resin can be cured thermally to create a cross-linked thermoset with excel.. |
|||
Shear Strength | 70.0 MPa | 10200 psi | ASTM D732 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK) AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea.. |
|||
Shear Strength | 70.0 MPa | 10200 psi | ASTM D732 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th.. |
|||
Shear Strength | 70.3 MPa | 10200 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and .. |
|||
Shear Strength | 70.0 MPa | 10200 psi | Safety factor of 10-20X is necessary in practice |
Saint-Gobain Vitreosil® Clear Fused Quartz Tubing Electrically fused quartz is recognized for its combination of purity, chemical inertness, physical stability, thermal shock resistance, high electrical resistivity, and high operating temperatures... |
|||
Shear Strength | 70.0 MPa | 10200 psi | Interlaminar shear strength; Vf=54%; L/d = 4. |
Toyobo Zylon® HM Fiber/Epoxy Matrix Unidirectional Composite Poly(p-phenylene-2,6-benzobisoxazole) (PBO) is a rigid-rod isotropic crystal polymer. Zylon is a new high performance fiber developed by TOYOBO using the latest material science and state of the ar.. |
|||
Shear Strength | 70.0 MPa | 10200 psi | IL; pr EN 2563 |
Hexcel® HexPly® 920CX-940-42% 125°C Curing Epoxy Matrix Intermediate modulus, 6K carbon, 5H satin, 285 g/m2Information provided by HexCel |
|||
Shear Strength | 70.0 MPa | 10200 psi | 0°, Short Beam |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, High Strength 6k carbon Balanced fabric 285 g/m2 Information provided by HexCel |
|||
Shear Strength | 70.0 MPa @Temperature 100 °C |
10200 psi @Temperature 212 °F |
In-Plane, Wet; EN6031 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber Information provided by HexCel |
|||
Shear Strength | 70.0 MPa | 10200 psi | 0º, Short Beam |
Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix, High Strength 12k Carbon Balanced Fabric 600 g/m2 Information provided by HexCel |
|||
Shear Strength | 70.0 - 84.0 MPa | 10200 - 12200 psi | IS 867-1963 |
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec.. |
|||
Shear Strength | 70.0 - 80.0 MPa | 10200 - 11600 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railwa.. |
|||
Shear Strength | 70.0 - 84.0 MPa | 10200 - 12200 psi | IS 867-1963 |
Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric .. |
|||
Shear Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATO 1510 Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthMedium copper adhesionColo.. |
|||
Shear Strength | 70.0 - 80.0 MPa | 10200 - 11600 psi | IS 867-1963 |
Amity Thermosets ATO 159 Phenolic Molding Glass/ inorganic Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |