Mechanical Properties Metric English Comments
Shear Strength 93.0 MPa
13500 psi
ASTM D732
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, at 50% RH  (d
AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di..
Shear Strength 93.1 MPa
13500 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire..
Shear Strength 93.1 MPa

@Thickness 15.7 mm
13500 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP313 Cotton Fabric
Description: Canvas phenolic laminate with molybdenum disulfide lubricant. Mechanical properties slightly lower than NP310.Thickness Tested: 0.062", 0.125" & 0.500"
Shear Strength 93.1 MPa

@Thickness 15.7 mm
13500 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP320 Cotton Fabric
Description: Fine weave (less than 4 ounce/square yard) cotton fabric commonly called linen, combined with phenolic resin to provide better machining than NP310. For smaller and more intricate shape..
Shear Strength 93.1 MPa

@Thickness 15.7 mm
13500 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP320E Cotton Fabric
Description: Similar to NP320 with improved moisture resistance. Suitable for electrical applications in moderate humidity conditions.Thickness Tested: 0.062", 0.125", and 0.500”
Shear Strength 93.1 MPa

@Thickness 15.7 mm
13500 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP347 Cotton Fabric
Description: Bleached canvas with high temperature phenolic resin with molybdenum disulfide lubricant. Low moisture absorption. Capable of 150°C continuous operation.Thickness Tested: 0.062", 0.1..
Shear Strength 93.1 MPa
13500 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber
KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS..
Shear Strength 93.0 MPa
13500 psi
Typical epoxy composite property; short-beam
Hexcel® HexTow™ PV42/850 Carbon Fiber
HexTow™ PV42/850 (HS-CP-3300) carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. This fiber has been designed for a..
Shear Strength 93.1 MPa
13500 psi
Ultimate
Ensinger TECAPEI® 20% Glass Reinforced, made from Ultem® 2200 PEI
TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in..