Mechanical Properties Metric English Comments
Shear Strength 53.0 MPa
7690 psi
ASTM D732
Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded  (discontinued **)
AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistan..
Shear Strength 53.0 MPa
7690 psi
ASTM D732
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded  (discontinued **)
AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti..
Shear Strength 53.0 MPa
7690 psi
Aardvark Polymers AARTEL® 820UV Acetal Copolymer Rotational Molding Resin
Aartel 820UV is a natural acetal copolymer with added UV stabilizers.Aartel 820UV is a low viscosity resin with excellent flow characteristics.Aartel 820UV is available in natural white and may be p..
Shear Strength 53.0 MPa

@Temperature 71.0 °C
7690 psi

@Temperature 160 °F
Compression interlaminar
Hexcel® HexPly® F155 Epoxy Resin, 220 Glass Fabric
Information provided by HexCel
Shear Strength 53.0 MPa

@Temperature 175 °C
7690 psi

@Temperature 347 °F
IL; Material as cured
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix
5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel
Shear Strength 53.0 MPa
7690 psi
0º, Short Beam
Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix, E-glass Balanced Fabric 600 g/m2
Information provided by HexCel