Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 53.0 MPa | 7690 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistan.. |
|||
Shear Strength | 53.0 MPa | 7690 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Shear Strength | 53.0 MPa | 7690 psi | |
Aardvark Polymers AARTEL® 820UV Acetal Copolymer Rotational Molding Resin Aartel 820UV is a natural acetal copolymer with added UV stabilizers.Aartel 820UV is a low viscosity resin with excellent flow characteristics.Aartel 820UV is available in natural white and may be p.. |
|||
Shear Strength | 53.0 MPa @Temperature 71.0 °C |
7690 psi @Temperature 160 °F |
Compression interlaminar |
Hexcel® HexPly® F155 Epoxy Resin, 220 Glass Fabric Information provided by HexCel |
|||
Shear Strength | 53.0 MPa @Temperature 175 °C |
7690 psi @Temperature 347 °F |
IL; Material as cured |
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix 5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel |
|||
Shear Strength | 53.0 MPa | 7690 psi | 0º, Short Beam |
Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix, E-glass Balanced Fabric 600 g/m2 Information provided by HexCel |