Mechanical Properties Metric English Comments
Shear Strength 58.0 - 70.0 MPa
8410 - 10200 psi
IS 867-1963
Amity Thermosets ATG 115 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic ..
Shear Strength 67.0 - 70.0 MPa
9720 - 10200 psi
IS 867-1963
Amity Thermosets ATI 101 Phenolic Molding Organic Filler, Injection Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit..
Shear Strength 60.0 - 70.0 MPa
8700 - 10200 psi
IS 867-1963
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium..
Shear Strength 55.0 - 70.0 MPa
7980 - 10200 psi
IS 867-1963
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App..
Shear Strength 60.0 - 70.0 MPa
8700 - 10200 psi
IS 867-1963
Amity Thermosets ATG 116 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- BlackMedium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic appliance ha..