Mechanical Properties Metric English Comments
Secant Modulus, TD 2.275 - 3.45 GPa
330.0 - 500 ksi
ASTM D882
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film  (discontinued **)
Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many ..
Secant Modulus, TD 2.275 - 3.28 GPa
330.0 - 476 ksi
ASTM D882
Honeywell Capran® Emblem™ 2530 Bi-Axially Oriented Nylon Film  (discontinued **)
Description: Capran® Emblem™ 2530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo..
Secant Modulus, TD 2.275 - 3.45 GPa
330.0 - 500 ksi
ASTM D882
Honeywell Capran® Emblem™ 1500 Clear Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr..
Secant Modulus, TD 2.275 - 3.45 GPa
330.0 - 500 ksi
ASTM D882
Honeywell Capran® Emblem™ 1500M M-Coated Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd..
Secant Modulus, TD 2.275 - 3.28 GPa
330.0 - 476 ksi
ASTM D882
Honeywell Capran® Emblem™ 2500 Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 2500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr..
Secant Modulus, TD 2.275 - 3.448 GPa
330.0 - 500.1 ksi
ASTM D882
Honeywell Capran® Emblem™ MT1500 Bi-Axially Oriented Nylon 6 Film
Description: Capran® Emblem™ MT1500 is a 0.60 mil (15 micron) biaxially oriented nylon 6 film with a metallized barrier coating well suited for high barrier packaging applications. Informati..
Secant Modulus, TD 2.275 - 3.282 GPa
330.0 - 476.0 ksi
ASTM D882
Honeywell Capran® Emblem™ MT2500 Bi-Axially Oriented Nylon 6 Film
Description: Capran® Emblem™ MT2500 is a 1.00 mil (25 micron) biaxially oriented nylon 6 film with a metallized barrier coating.Applications: Capron® Emblem™ MT2500 is well suited fo..
Secant Modulus, TD 2.275 - 3.241 GPa
330.0 - 470.1 ksi
ASTM D882
Honeywell Capran® Oxyshield™ OBS Monoaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film
Description: Oxyshieldâ„¢ Oriented Barrer is a 0.60 mil (15 micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier through a bro..
Copyright © lookpolymers.com All Rights Reserved