Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 1300 - 1800 MPa | 189000 - 261000 psi | Average value: 1630 MPa Grade Count:8 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Creep Modulus, 1000 hours | 1300 MPa | 189000 psi | ISO 899-1 |
Lanxess Pocan® B 1505 000000 PBT PBT, non-reinforced, injection molding, extrusion |
|||
Tensile Creep Modulus, 1000 hours | 1300 MPa | 189000 psi | ISO 899 |
BASF Ultraform H 2320 006 Q600 POM Ultraform H2320 006 is a high-molecular-weight grade of POM for injection molding. It conforms to FDA requirements of 21 CFR 177.2470. |
|||
Tensile Creep Modulus, 1000 hours | 1300 MPa | 189000 psi | ISO 899-1 |
BASF Ultraform H 4320 Q600 POM Ultraform H4320 Q600 is an extrusion POM high molecular weight grade. This grade enables high extrusion rates with thick-walled product. It also exhibits high thermal stability and a low tendency .. |
|||
Tensile Creep Modulus, 1000 hours | 1300 MPa | 189000 psi | ISO 899 |
BASF Ultraform N 2310P Q600 POM Ultraform N2310P Q600 is a general-purpose injection molding POM grade containing special lubricant. Low frictional coefficient giving extremely low wear with otherwise unaltered mechanical propert.. |
|||
Tensile Creep Modulus, 1000 hours | 1300 MPa | 189000 psi | ISO 899-1 |
BASF Ultraform® S2320 003 PRO BK 00120 POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Tensile Creep Modulus, 1000 hours | 1300 MPa | 189000 psi | ISO 899-1 |
BASF Ultraform® S2320 003 PRO POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Tensile Creep Modulus, 1000 hours | 1300 MPa | 189000 psi | |
Arkema Group Oroglas® SG 7 Acrylic, Gamma Radiation Resistant
(discontinued **) OROGLAS SG 7 is special Gamma - radiation - resistant formulation designed for use in medical devises.OROGLAS SG 10 maintains exceptional clarity after 5 megarads of Gamma radiation with no adverse .. |