Polymer Property : Tensile Creep Modulus, 1000 hours = 1800 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 700 - 1800 MPa
102000 - 261000 psi
Average value: 1260 MPa Grade Count:20
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Tensile Creep Modulus, 1000 hours 650 - 1800 MPa
94300 - 261000 psi
Average value: 1460 MPa Grade Count:8
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
Tensile Creep Modulus, 1000 hours 1300 - 1800 MPa
189000 - 261000 psi
Average value: 1630 MPa Grade Count:8
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Tensile Creep Modulus, 1000 hours 1200 - 1800 MPa
174000 - 261000 psi
Average value: 1580 MPa Grade Count:10
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Tensile Creep Modulus, 1000 hours 1000 - 1800 MPa
145000 - 261000 psi
Average value: 1580 MPa Grade Count:4
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..