NOVA Chemicals Sclair® 2111 LLDPE Injection Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 2111 LLDPE Injection Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good processability, Excellent impact resistance, Excellent flexibility and freedom from warpageApplications: Automotive splash-guards, Large containers, Closures and lids for food applicationsAdditives: AntioxidantInformation provided by NOVA Chemicals.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D792
Environmental Stress Crack Resistance <= 10 hour
<= 10 hour
F<sub>50</sub>; Condition A, 100% Igepal; ASTM D1693
Melt Flow 19 g/10 min

@Load 2.16 kg,
Temperature 190 °C
19 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 52
52
ASTM D2240
Tensile Strength, Yield 10.0 MPa
1450 psi
50 mm/min; ASTM D638
Elongation at Break 850 %
850 %
50 mm/min; ASTM D 638
Flexural Modulus 0.345 GPa
50.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 170 - 215 °C
338 - 419 °F