Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil PP7694E2 Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP7694E2 Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A high crystallinity, medium impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for applications requiring long-term heat-aging resistance and excellent finished part appearance.Availability: North America and South America Features:Good ColorabilityGood ProcessabilityGood Thermal Aging ResistanceHigh Impact ResistanceHigh StiffnessLow WarpageUses: Appliance ComponentsAppliancesConsumer ApplicationsTool/Tote BoxProcessing Method: Injection Molding and CompoundingInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 19 g/10 min

@Load 2.16 kg,
Temperature 230 °C
19 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.7 MPa
3580 psi
2 in/min; ASTM D638
Elongation at Yield 5.6 %
5.6 %
2 in/min; ASTM D638
Flexural Modulus 1.27 GPa
184 ksi
1% secant, 0.05 in/min.; ASTM D790
1.45 GPa
210 ksi
1% secant, 0.5 in/min; ASTM D790B
Izod Impact, Notched 1.39 J/cm
2.60 ft-lb/in
ASTM D256
Gardner Impact 23.7 J

@Thickness 3.17 mm,
Temperature -30.0 °C
17.5 ft-lb

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
216 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 204 - 232 °C
399 - 450 °F
Typical
Copyright © lookpolymers.com All Rights Reserved