Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.780 GPa | 113 ksi | Secant; ASTM D3350 |
NOVA Chemicals Novapol® HD-2100-U MDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | 1% Strain Value from rotomolded samples; ASTM D790 |
NOVA Chemicals Novapol® TR-0735-U Hexene MDPE Rotational Molding Resin Good impact resistance, Excellent processabilityApplications: Toys, Complex custom parts, Home and garden items, MailboxesAdditives: Processing antioxidants, UV stabilizersInformation provided by NO.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | ASTM D790 |
NOVA Chemicals Novapol® TR-0735-UG Hexene MDPE Rotational Molding Resin Features: Good impact properties Excellent processabilityNSF listed for Stds. 14, 24 and 61 Applications: ToysComplex custom partsHome and garden itemsMailboxesInformation provided by Nova Chemicals.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | Secant; ASTM D3350 |
NOVA Chemicals Novapol® HD-2100-A MDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.779 GPa | 113 ksi | ASTM D790 |
Formosa Plastics Formolene® HL3721 Sheet and Thermoforming HDPE
(discontinued **) Medium Density Hexene CopolymerApplications: Geomembranes, gas and chemical tank containment liners, landfill liners.Formolene HL3721 is tailored for extrusion applications requiring good processabi.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | 1% Strain Value from rotomolded samples; ASTM D790 |
NOVA Chemicals Novapol® PR-0636-UG Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | 1% Strain Value from rotomolded samples; ASTM D790 |
NOVA Chemicals Sclair® TD-7915-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |
|||
Flexural Modulus | 0.779 - 1.55 GPa | 113 - 225 ksi | Average value: 1.18 GPa Grade Count:18 |
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is .. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax PF511 Polypropylene Homopolymer, Radiation Resistant Primary Processing Method: Injection MoldingKey Features: high melt flow, radiation-resistant polypropylene homopolymer resin, excellent retention of physical properties and color after radiation st.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | ASTM D790 |
LG Chemical LUCEL ST-550 Ultra High Impact POM, Unreinforced LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GM 5010 T2 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GM 7746 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | ASTM D790 |
UBE 7128B Nylon 6/12 Copolymer Description: UBESTA Nylon 12 CopolymerInformation provided by UBE. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | ASTM D790 |
Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer Benefits: good processability, excellent melt strength, broad fusion range, outstanding stress cracking resistanceApplications: geomembrane, gas and chemical containment liners, landfill linersInfor.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, Conditioned Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | 1% Strain Value from rotomolded samples; ASTM D790 |
NOVA Chemicals Sclair® TD-7915-U Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, Conditioned Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Flexural Modulus | 0.780 GPa | 113 ksi | 1% Strain Value from rotomolded samples; ASTM D790 |
NOVA Chemicals Novapol® PR-0636-U Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |