Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Molded
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Benefits: good processability, excellent melt strength, broad fusion range, outstanding stress cracking resistanceApplications: geomembrane, gas and chemical containment liners, landfill linersInformation provided by Chevron Phillips Chemical Company
Physical Properties Metric English Comments
Density 0.937 g/cc
0.0339 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 1500 hour

@Temperature 50.0 °C
>= 1500 hour

@Temperature 122 °F
Condition B; ASTM D 1693
High Load Melt Index 21 g/10 min

@Load 21.6 kg,
Temperature 190 °C
21 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638 Type IV
Elongation at Break >= 600 %
>= 600 %
ASTM D638 Type IV
Flexural Modulus 0.780 GPa
113 ksi
ASTM D790
Processing Properties Metric English Comments
Processing Temperature 193 - 210 °C
379 - 410 °F
stock temperature