Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Novapol® HD-2100-U MDPE Extrusion Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded , MDPE
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® HD-2100-U MDPE Extrusion Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 5000 hour
>= 5000 hour
F0, Condition C, ASTM D1693, 100% Igepal
Melt Flow 0.14 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.14 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM D638
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D638
Tensile Modulus 0.800 GPa
116 ksi
Secant; ASTM D638
Flexural Modulus 0.780 GPa
113 ksi
Secant; ASTM D3350
Thermal Properties Metric English Comments
CTE, linear 140 µm/m-°C

@Temperature 20.0 °C
77.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 128 °C
262 °F
ASTM D3417
Vicat Softening Point 119 °C
246 °F
ASTM D1525
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D696
Processing Properties Metric English Comments
Melt Temperature 195 - 225 °C
383 - 437 °F