Polymer Property : Flexural Modulus = 15.8 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 15.8 GPa
2290 ksi
ASTM D790
Quantum Composites QC-7753 50% Glass Fiber Reinforced Polyester SMC
QC-7753 is a polyester engineered structural composite molding compound that is designed for applications requiring high strength, fire retardant properties, and resistance to elevated temperatures...
Flexural Modulus 15.8 GPa
2290 ksi
ASTM D790
LATI LARPEEK 10 K/20 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK)  (Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
Flexural Modulus 15.8 GPa
2290 ksi
ASTM D790
Solvay Specialty Polymers Kadel® E-1230 Polyketone  (discontinued **)
Electrical Conductor. High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, p..
Flexural Modulus 15.8 GPa
2290 ksi
ASTM D790
Quantum Composites QC-8100 60% Glass Fiber Vinyl Ester SMC  (discontinued **)
QC-8100 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and corrosion resistance. Form and Colors = Rolled Shee..
Flexural Modulus 15.8 GPa
2290 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA12
LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
Flexural Modulus 15.8 GPa
2290 ksi
ISO 178
Solvay Specialty Polymers Kalix® 2955 Polyamide, High Performance (HPPA), Glass Fiber
Kalix® 2955 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is specifically formulated for high strength and stiffness applications where ..