Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.30 - 1.70 GPa | 189 - 247 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_4310 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Flexural Modulus | 1.30 - 1.70 GPa | 189 - 247 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_4410 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Flexural Modulus | 1.30 - 1.70 GPa | 189 - 247 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_4510 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Flexural Modulus | 1.30 - 1.70 GPa | 189 - 247 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_4710 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Flexural Modulus | 1.40 - 1.70 GPa | 203 - 247 ksi | |
Reliance Industries Polypropylene Homopolymer Typical properties of Reliance - Repol Polypropylene gradesInformation provided by Reliance Industries |
|||
Flexural Modulus | 1.60 - 1.70 GPa | 232 - 247 ksi | ASTM D790 |
Loxim 811 02T HB Polypropylene Compound, 10% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Flexural Modulus | 1.50 - 1.70 GPa | 218 - 247 ksi | ASTM D790 |
Loxim 820 02C HB Polypropylene Compound, 20% Calcite Filled, Flame Retardant Information provided by Loxim Industries |