Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 18.5 GPa | 2680 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1023 Polyarylamide (PARA)
(discontinued **) Ixef 1023 is a 50% glass-fiber reinforced, UV stabilized polyarylamide for interior applications, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resis.. |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1028 Polyarylamide (PARA)
(discontinued **) Ixef 1028 is a laser printable, 50% glass-fiber reinforced polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1028.. |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | DIN 53 457 |
Albis Plastics Tedur® L 9521-1 PPS, 60% Glass Fiber/Mineral
(discontinued **) Extremely Rigid. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Sockets, Plugs and HandlesProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperatur.. |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AE-8950 Polyphthalamide (PPA), 50% Glass Fiber Amodel® AE-8950 is a 50% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep .. |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA), 50% Glass Fiber Amodel® DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o.. |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good.. |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® FC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® FC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® HC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® HC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon DEF13 PC LNP* Stat-kon* DEF13 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP IF00C PA6.12 LNP* THERMOCOMP* IF00C is a compound based on Nylon 6/12 resin containing 60% Glass Fiber. |
|||
Flexural Modulus | 18.48 GPa | 2680 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66 LNP THERMOCOMP* RF00C is a compound based on Nylon 66 resin containing 60% Glass Fiber. |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | dry; ISO 178 |
DSM Stanyl® TW200B6 PA46-CF30 30% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 CF30 HWCP 30% Carbon Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 CF 30 HWCP 30% Carbon Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 18.5 GPa | 2680 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA)
(Unverified Data**) Ixef 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 102.. |
|||
Flexural Modulus | 18.5 GPa @Temperature 23.0 °C |
2680 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA)
(Unverified Data**) Amodel DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th.. |