Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AE-8950 Polyphthalamide (PPA), 50% Glass Fiber

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AE-8950 Polyphthalamide (PPA), 50% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® AE-8950 is a 50% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Heat Resistance; High Stiffness; High Strength; High Temperature Strength; Low Moisture Absorption; Non-CorrosiveUses: Automotive Electronics; Connectors; Electrical Parts; Electrical/Electronic ApplicationsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Additional Properties: Flexural Strain - ISO 178 2.3 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
Filler Content 50 %
50 %
Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength at Break 280 MPa
40600 psi
ISO 527-2
Elongation at Break 2.1 %
2.1 %
ISO 527-2
Tensile Modulus 19.8 GPa
2870 ksi
ISO 527-2
Flexural Strength 400 MPa
58000 psi
ISO 178
Flexural Modulus 18.5 GPa
2680 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
Type 1, Notch A; ISO 180
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
Type 1, Edgewise; ISO 179
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
Type 1, Edgewise; ISO 179
Thermal Properties Metric English Comments
Melting Point 325 °C
617 °F
ISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 300 °C
572 °F
Unannealed; ISO 75-2/A
Glass Transition Temp, Tg 135 °C
275 °F
DSC
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Processing Properties Metric English Comments
Rear Barrel Temperature 316 - 330 °C
601 - 626 °F
Middle Barrel Temperature 316 - 330 °C
601 - 626 °F
Front Barrel Temperature 324 - 340 °C
615 - 644 °F
Melt Temperature 330 - 350 °C
626 - 662 °F
Mold Temperature 150 - 165 °C
302 - 329 °F
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Moisture Content 0.030 - 0.060 %
0.030 - 0.060 %
Suggested Max
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black
Form Pellets
Processing Technique Injection Molding