Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.69 - 3.24 GPa | 390 - 470 ksi | ASTM D790 |
Proto3000 Accura® 55 Plastic Stereolithography (SLA) Prototyping Polymer Simulate the look and feel of molded ABS with this tough and versatile plastic.Features:Durable and rigid materialLook and feel of molded ABSHigh accuracy with less distortionHigh production speedLo.. |
|||
Flexural Modulus | 1.86 - 3.24 GPa | 270 - 469 ksi | Average value: 2.80 GPa Grade Count:8 |
Overview of materials for Acrylic, High Flow, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app.. |
|||
Flexural Modulus | 2.69 - 3.24 GPa | 390 - 470 ksi | ASTM D790 |
3D Systems Accura® 55 Plastic for SLA® Systems Simulate the properties and appearance of molded ABS. For use with solid-state stereolithography (SLA®) systems.ApplicationsAutomotive interior componentsShort-run production partsElectronic compon.. |