Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.31 GPa | 480 ksi | Tangent; ASTM D790 |
RheTech Products G20P100-00 20% Glass Fiber Reinforced Polypropylene, Natural Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers PC-1010 Description: Polycarbonate, 10% Glass Filled BlackInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Niche Polymer PPCG20BK Copolymer PP, 20% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Quantum PEI - Ultem® Information provided by Quantum Advanced Engineering Plastics |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | Tangent; ASTM D790 |
RheTech Products G20P100-601 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUA5) Dark Graphite Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Quantum Nylon 6/6 MoS2 Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790-1 |
Ineos Styrenics Polystyrene 168M (NAFTA) High heat, high molecular weight general purpose polystyrene with low crystal clarity. It offers high stiffness for extrusion/thermoforming applications, especially for the food packaging.Informati.. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Techmer ES Luriblend® PA6 ML3 BK Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(3%)Features: Good Wear Resistance, Low Friction, Heat Stabilized and LubricatedAppearance: Black.. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer (Asia Pacific) LNP* THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D 790 |
Styrolution PS 1621 GPPS Easy flow material with excellent moldabilityExcellent clarity and set-up timeInformation provided by Styrolution |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D 790 |
Styrolution PS 2600/2601 GPPS Foam extrusionLow residual styrene monomer contentModerate heat resistanceGood balance of strength and ease of processingUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolut.. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D 790 |
Styrolution PS 3190/3191 GPPS Low residual styrene monomer contentGood balance of flow and set-up propertiesInformation provided by Styrolution |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D 790 |
Styrolution PS 2610 GPPS Extruded packaging; Thermoforming applicationsExcellent toughnessHigh melt strengthGood flow and processabilityInformation provided by Styrolution |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Chase Plastics CP Pryme® PC310GR Polycarbonate (Utility Grade), 10% Glass Fiber Reinforced, Mold Release Information provided by Chase Plastics. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFLAM™ FPP 1007F Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007F is a 40% talc filled homopolymer polypropylene compound that utilizes FDA compliant raw materials.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Westlake Plastics Tempalux® Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Westlake Plastics Tempalux® Polyetherimide For Medical Applications Medical grade Tempalux is made from Ultem® polyetherimide resin, an amorphous thermoplastic which exhibits excellent resistance to a wide range of chemicals and disinfectants. Ultem maintains its .. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFLAM™ FPP 1007F Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007F is a 40% talc filled homopolymer polypropylene compound that utilizes FDA compliant raw materials.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | Tangent; ASTM D790 |
Washington Penn Polypropylene Copolymer 20% Glass Reinforced, 15 MFI Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. .. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | Tangent; ASTM D790 |
RheTech Products G20P100-406 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUEA) Midnight Black Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |