Polyram PlusTek PB351I6 Nylon 6, 30% Glass Fiber and Mineral

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Polyram
Trade Name PlusTek
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PB351I6 Nylon 6, 30% Glass Fiber and Mineral.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% glass fiber and mineral reinforced polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM-D638
Elongation at Break 2.5 %
2.5 %
ASTM-D638
Tensile Modulus 3.70 GPa
537 ksi
ASTM-D790
Flexural Strength 75.0 MPa
10900 psi
ASTM D790
Flexural Modulus 4.10 GPa
595 ksi
ASTM-D790
Izod Impact, Notched 0.450 J/cm

@Temperature 23.0 °C
0.843 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F