Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.70 GPa | 827 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PC 69 GF 35 FRT 4 Polypropylene Copolymer, 35% Glass Fiber, Halogen Free and Phosphor Free Flame Retardant FeaturesModified copolymer PP for injection moulding, chemically reinforced with 35% glass fiber, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. I.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178, ASTM D790 |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Flexural Modulus | 5.70 GPa @Temperature 60.0 °C |
827 ksi @Temperature 140 °F |
ASTM D790 |
LATI LARIL 13 G/20-V1 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM D790 |
Qualchem Danaprop PP1GF-30 Polypropylene, 30% Glass Fiber Polypropylene (co-polymer) reinforced with glass fiberInformation provided by Qualchem Zrt. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM D790 |
NOVA Chemicals Dylark® 480P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 20 FN20 DUS013 000000 Nylon 6, 20% Glass Fiber PA 6, 20% glass fibers, injection molding, halogen-free flame retardantInformation provided by LANXESS. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PX7446 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM D790 |
Solvay TECHNYL® C 52G4 MZ25 PA6, 25% mineral filler, DRY Description: TECHNYL® C 52G4 MZ25 is a 25% mineral reinforced melamine cyanurate flame retarded polyamide 6.This product is heat stabilized and is suitable for injection molding. This product is .. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East) VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS (Asia Pacific) LNP* Stat-loy* AF306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Antistat. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM D790 |
Techmer ES Plaslube® J-1/20/MS/5 NAT PA66 |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Polyplastics Duranex® 361SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM-D790 |
Polyram RamLloy PA917G4 PP/NYLON 66 alloy, 20% Glass Fiber 20% glass fiber reinforced PA66/PP alloy with reduced water absorption, dimensional stability and UV stabilized for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Wellman Wellamid® MR409 22H-N 40% Mineral Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM D790 |
Unitika UG-100-30 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
DuPont Performance Polymers Sorona® 3015GV BK001 Polytrimethylene Terephthalate (PTT) 15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3015GV BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% based .. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | cond.; ISO 178 |
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
BASF Ultramid® FRee B3U31G4 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 436 Glass/Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.20% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 413 Glass Reinforced, Polycarbonate/Polyester Alloy, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher .. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM D790 |
PolyOne Lubri-Tech™ ES-20GF/15T Polyethersulfone - 20% Glass Fiber Reinforced - 15% PTFE Lubricated
(disconti Data provided by PolyOne. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® VX4920 PBT (Europe-Africa-Middle East) VALOX VX4920 is a 20% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |
|||
Flexural Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe.. |