Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Water Absorption 0.60 %
0.60 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength at Break 108 MPa
15700 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Modulus 5.70 GPa
827 ksi
ASTM D790
Compressive Strength 172 MPa
25000 psi
ASTM D695
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
ASTM D256