Polymer Property : Flexural Modulus = 502 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.46 GPa
502 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycolac® INP562 ABS
SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Flexural Modulus 3.46 GPa
502 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN
SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Flexural Modulus 3.46 GPa
502 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycolac® INP563 ABS
SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Flexural Modulus 3.46 GPa
502 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycolac® INP563 ABS+SAN
SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Flexural Modulus 3.46 GPa
502 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycolac® INP564 ABS
SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Flexural Modulus 3.46 GPa
502 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycolac® INP564 ABS+SAN
SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Flexural Modulus 3.46 GPa
502 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycolac® INP572 ABS
High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro..
Flexural Modulus 3.46 GPa
502 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycolac® INP572 ABS+SAN
High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro..
Flexural Modulus 3.46 GPa
502 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp KB004 Acetal Copolymer
LNP THERMOCOMP* KB004 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 3.46 - 10.62 GPa

@Temperature -40.0 - 200 °C
502 - 1540 ksi

@Temperature -40.0 - 392 °F
Average value: 5.77 GPa Grade Count:2
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..