Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.70 - 7.60 GPa | 247 - 1100 ksi | Average value: 2.66 GPa Grade Count:15 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Modulus | 3.30 - 7.60 GPa | 479 - 1100 ksi | Average value: 4.83 GPa Grade Count:4 |
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Flexural Modulus | 0.750 - 7.60 GPa | 109 - 1100 ksi | Average value: 2.49 GPa Grade Count:236 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Flexural Modulus | 2.83 - 7.60 GPa | 410 - 1100 ksi | Average value: 4.61 GPa Grade Count:25 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |