Flexural Modulus 3.20 - 8.96 GPa
464 - 1300 ksi
Average value: 5.39 GPa Grade Count:34
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Flexural Modulus 2.55 - 8.96 GPa
370 - 1300 ksi
Average value: 5.97 GPa Grade Count:14
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Flexural Modulus 4.83 - 8.96 GPa
700 - 1300 ksi
Average value: 6.48 GPa Grade Count:15
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E..
Flexural Modulus 6.89 - 8.96 GPa
1000 - 1300 ksi
ASTM D790
Premix Premi-Glas® 1201-10 Polyester SMC  (discontinued **)
Premi-Glas® 1201-10 is a 10% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS..
Flexural Modulus 7.58 - 8.96 GPa
1100 - 1300 ksi
Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester
BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where hig..
Flexural Modulus 7.58 - 8.96 GPa
1100 - 1300 ksi
Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound
BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding..
Flexural Modulus 7.58 - 8.96 GPa
1100 - 1300 ksi
Bulk Molding Compounds BMC T40(18)V0 Die Casting Replacement Grade Molding Compound
BMC T40(18)V0 is a lower cost version of BMC T40(18) where a UL 5V rating is not necessary.