Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.590 GPa
85.6 ksi
ASTM D790
NOVA Chemicals Sclair® 35BP HDPE Extrusion Resin, 2.2% Carbon Black Filled  (discontinued **)
Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi..
Flexural Modulus 0.590 - 0.810 GPa
85.6 - 117 ksi
Average value: 0.673 GPa Grade Count:8
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m..
Flexural Modulus 0.590 GPa
85.6 ksi
2% secant; ASTM D790-02
Ipiranga Petrochem MB 0434 LS-L MDPE
IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye..
Flexural Modulus 0.590 GPa
85.6 ksi
2% secant; ASTM D790-02
Ipiranga Petrochem MB 0435 MDPE
IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye..
Flexural Modulus 0.590 GPa
85.6 ksi
ISO 178
Borealis Casico™ FR4805 Non Halogen Flame Retardant Compound for Sheathing Energy Cables
Casico FR4805 is a thermoplastic, non-halogen containing natural jacketing compound. It combines high mechanical strength and toughness with flame retardancy. The composition of Casico FR4805 is b..
Flexural Modulus 0.590 GPa
85.6 ksi
ASTM D790
Covestro Bayflex® 180 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o..
Flexural Modulus 0.590 GPa
85.6 ksi
ASTM D790
Asahi Glass Fluon® P-65P PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Flexural Modulus 0.590 GPa
85.6 ksi
ASTM D790
Asahi Glass Fluon® P-805UP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Flexural Modulus 0.590 GPa
85.6 ksi
ASTM D790
NOVA Chemicals Sclair® 35BPM MDPE Extrusion Resin, 2.2% Carbon Black Filled  (discontinued **)
Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi..
Flexural Modulus 0.590 - 0.840 GPa
85.6 - 122 ksi
Average value: 0.694 GPa Grade Count:9
Overview of materials for Medium Density Polyethylene (MDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max..