Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 110 kN/m | 628 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Vyram™ 9103-54 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 110 kN/m | 630 pli | Die C; ASTM D624 |
Mearthane Durethaneâ„¢ S DS-560D Solid Polyurethane Elastomer TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM D624 |
GRECO ISOTHANE 1095AF Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject.. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM D624 |
GRECO ISOTHANE 1190A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tear Strength | 110 kN/m | 628 pli | ISO 34-1B |
Lubrizol Advanced Materials Pearlthane® D91T86 Thermoplastic Polyurethane Type : Pearlthane® D91T86 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties... |
|||
Tear Strength | 110 kN/m | 628 pli | ISO 34B |
Huntsman AVALON® 90 AK Thermoplastic Polyurethane Introduction: AVALON 90 AK is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same har.. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM D624 |
LyondellBasell Hifaxâ„¢ ETA-3131E Thermoplastic Olefin Resin Key Features: fractional melt flow, medium modulus, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good practical impact, good processabilityApplications: molded.. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM D624 |
LyondellBasell Hifaxâ„¢ ETA-5061 Thermoplastic Olefin Resin Key Features: fractional melt flow, medium low modulus, blow molding grade thermoplastic olefin resin, flexible, good impact resistance, good processabilityApplications: automotive ductwork, convolu.. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM D624 |
LyondellBasell Hifaxâ„¢ ETA-5081 Thermoplastic Olefin Resin Key Features: fractional melt flow, medium modulus, blow molding grade thermoplastic olefin resin, flexible, good impact resistance, good processabilityApplications: automotive ductwork, convoluted .. |
|||
Tear Strength | 110 kN/m | 630 pli | ASTM D624 |
LyondellBasell Hifaxâ„¢ RTA3263EUV Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263EUV fractional melt flow, 1,500 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent com.. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM D624 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-2185 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM D624 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM D624 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tear Strength | 110 kN/m | 628 pli | Die C; ASTM D624 |
Covestro Bayflex® 110-50 Polyurethane Elastomeric RIM, 15% Milled Glass Reinforced, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Tear Strength | 110 kN/m | 628 pli | Die C; ASTM D624 |
Covestro Bayflex® 110-50 Polyurethane Elastomeric RIM, 15% Mineral Filled, MDI-based 2-Component Liquid System Mineral filler is RRIMGLOS® 10013. 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialSc.. |
|||
Tear Strength | 110 kN/m | 628 pli | Die C; ASTM D624 |
Covestro Bayflex® 110-80 Polyurethane Elastomeric RIM, 15% Milled Glass Reinforced, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Tear Strength | 110 kN/m | 628 pli | parallel; ISO 34-1 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |
|||
Tear Strength | 110 kN/m | 628 pli | Die C; ASTM D412 |
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tear Strength | >= 110 kN/m | >= 628 pli | ISO 34 |
Austin Novel Materials Texalan® 290A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tear Strength | >= 110 kN/m | >= 628 pli | ISO 34 |
Austin Novel Materials Texalan® 772D PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM D624 |
BASF Elastollan® M80A55 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM D624 |
BASF Elastollan® M88A55 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1290 Polyester Based TPU Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM D624 |
LyondellBasell Hifax™ CB235 Thermoplastic Olefin Resin Key Features: medium high melt flow, medium high modulus, paintable thermoplastic olefin resin, excellent impact and stiffness balance, good dimensional stability, excellent processability, good pai.. |
|||
Tear Strength | 110 kN/m | 628 pli | ASTM D624 |
LyondellBasell Hifax™ ETA-3163UV Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, UV-stabilized thermoplastic olefin resin, excellent impact and stiffness balance, excellent weatherability, good processabilityApplications: mold.. |
|||
Tear Strength | 110 kN/m | 625 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 37-034 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledUV StabilizedApplications:General PurposeMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First Choic.. |