Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 26.0 kN/m | 148 pli | ISO 34-1 |
PolyOne OnFlex™ S EH 70A-3S7004 Thermoplastic Elastomer (TPE) OnFlex™-S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Tear Strength | 26.0 kN/m | 148 pli | D624 |
Polykemi AB POLYelast TPE Z800 SHF Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tear Strength | 26.0 kN/m | 148 pli | D624 |
Polykemi AB POLYelast TPE Z800 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tear Strength | 25.9 kN/m | 148 pli | Die-C; ASTM D624 |
Northstar Polymers MPA-A30B Mold-Making Resin MPA-A30B is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Tear Strength | 25.9 kN/m | 148 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Vyram™ 9101-65 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Tear Strength | 25.9 kN/m | 148 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 40-HR-9 TPE Product Description: StarTUFF TF 40-HR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Tear Strength | 25.9 kN/m | 148 pli | Initial Tear Strength; ASTM D624-91 Die B |
Saint-Gobain Versilicâ„¢ SPX-50 High Strength Silicone Tubing Formulation Description: Versilicâ„¢ SPX-50: Peroxide-cured Versilicâ„¢ High-Strength Silicone Tubing is designed for use in applications where flexibility, resiliency and durability are required. Its s.. |
|||
Tear Strength | 26.0 kN/m | 148 pli | |
Trelleborg R574 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 26.0 kN/m | 148 pli | |
Trelleborg R642 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 26.0 kN/m | 148 pli | |
Trelleborg R644 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 25.9 kN/m | 148 pli | Die C |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 10.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Tear Strength | 26.0 kN/m | 148 pli | ASTM D624 |
ELASTO UK Dryflex® 650600 TPE, Improved Compression Set and High Temperature Resistance, 60A Hardness The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi.. |
|||
Tear Strength | 25.9 kN/m | 148 pli | 73°F, Die C, Across Flow; ASTM D624 |
ExxonMobil Santoprene® 121-75M100 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult .. |
|||
Tear Strength | 25.9 kN/m | 148 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Santoprene® 8271-75 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Tear Strength | 26.0 kN/m | 148 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 5565 ASTM D3568 FormulationNordel® IP 5565 |
|||
Tear Strength | 25.9 kN/m | 148 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Vyram™ 9201-65 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Tear Strength | 25.9 kN/m | 148 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 5 Industrial PTFE-Coated Glass Description: Chemfab® Industrial Series products are multi-purpose, non-porous, medium-resin content, PTFE-coated fiberglass fabrics. Applications include release sheets, packaging, composites, gas.. |
|||
Tear Strength | 25.9 kN/m | 148 pli | Die C |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 10.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Tear Strength | 26.0 kN/m | 148 pli | ISO 34-B |
AlphaGary Evoprene™ GC 5658 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |