Mechanical Properties Metric English Comments
Flexural Strength 276 MPa

@Temperature 216 °C
40000 psi

@Temperature 420 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac..
Flexural Strength 276 MPa

@Temperature 93.3 °C
40000 psi

@Temperature 200 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Flexural Strength 276 MPa

@Temperature 216 °C
40000 psi

@Temperature 420 °F
Dry, Autoclave with Post-Cure; ASTM D790
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Flexural Strength 276 MPa

@Temperature 177 °C
40000 psi

@Temperature 350 °F
Dry, Autoclave; ASTM D790
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Flexural Strength 276 MPa

@Temperature 260 °C
40000 psi

@Temperature 500 °F
Dry; 325°F Autoclave Cured; ASTM D790
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Flexural Strength 276 MPa

@Thickness 1.57 mm
40000 psi

@Thickness 0.0620 in
CW
Industrial Laminates/Norplex NP841 Glass Fabric  (discontinued **)
Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: ..
Flexural Strength 276 MPa

@Thickness 1.57 mm
40000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP424 Laminate
Description: Composite material composed of woven glass fabric surfaces and paper core combined with epoxy resin. Primarily used in the printed circuit board industry. Easy punching and excellent el..
Flexural Strength 276 MPa

@Temperature -40.0 °C
40000 psi

@Temperature -40.0 °F
ASTM D790
DuPont Performance Polymers Rynite® 830ER NC010 PET
Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers